How to solve the deformation of 1.5mm алюминий парағы in processing?
The solution of алюминий парағы deformation is as follows:
1. Artificial aging before processing.
2. During machining, it is divided into rough machining and finishing machining. After the rough machining is completed, it is left for 8 дейін 12 hours to release stress.
3. When processing thin sheets, it is necessary to press on the table.
4. Control the cutting temperature so that the temperature rise influence area is as small as possible.
5. For complex shapes, orthopedics after processing.
The above is the solution to the deformation of the алюминий парағы processing shared by the editor. During the алюминий парағы өңдеу, pay attention to the above points to avoid the problem of aluminum sheet processing deformation.